Felix produces composite structures and laminates that are more than stagnant for the medical applications...
Felix produces composite structures and laminates that are more than stagnant for the medical applications. Our products are functional on the job. Most of our products are used in disposable medical articles such as gowns, table covers, absorbent materials and such. Since the medical fabrics are very complex and require lots of expertise, we work with best sub suppliers in order to deliver the customer expectation into reality. We value the customer`s expectations and needs beyond our capabilities and push ourselves to deliver the required results.
We use different kinds of medical fabrics such as SMS, Melt blown and Viscose Dry laid composites in our production scope. SMS ( Spunbond/Meltblown/Spunbond) nonwoven fabrics provides excellent barrier properties alone. Lamination of such nonwovens with Breathable or non-breathable film brings out extraordinary functionality and values such as complete impermeability against liquid penetration, while letting the fabric to breath. Melt blown and viscose dry laid nonwovens laminated to the breathable or non-breathable films are used for absorbent applications, where the liquid is kept on the absorbent material, while the film restricts leakage.
Double layer or Triple layer Breathable medical laminates | ||
Production technology | : | Hot melt lamination |
Input raw material | : | Double layer laminate: Nonwoven / Breathable film |
: | Triple layer laminate: Nonwoven / Breathable film / Nonwoven | |
Laminate Weight | : | 40 - 110 g/m2 |
WVTR | : | 500 - 9.500 grams/m2/24hr (ASTM E96- 2000 Desiccant) |
Double layer or Triple layer Non-Breathable medical laminates | ||
Production technology | : | Hot melt lamination |
Input raw material | : | Double layer laminate: Nonwoven/Breathable film |
: | Triple layer laminate : Nonwoven / Breathable film / Nonwoven | |
Laminate Weight | : | 40 - 200 g/m2 |
WVTR | : | 500 - 9.500 grams/m2/24hr (ASTM E96- 2000 Desiccant) |
Absorbent Non-Breathable medical laminates | ||
Production technology | : | Hot melt lamination |
Input raw material | : | Nonwoven / Breathable film |
Laminate Weight | : | 60 - 300 g/m2 |
Absorbency | : | up to % 800 |